We are leading manufacturer and stockist of Haynes 25 in China.
Haynes 25 Technical Data Sheet
Haynes 25 Chemical Composition Limits | ||||||||||
Weight% | C | P | Si | Ni | W | Mn | S | Cr | Co | Fe |
Alloy L-605 | 0.05 - 0.15 | 0.040 max | 0.40 max | 9.0 - 11.0 | 14.0 - 16.0 | 1.0 - 2.0 | 0.030 max | 19.0 - 21.0 | Bal | 3.0 max |
Udimet Alloy L-605 / Haynes 25 is a solid solution strengthened cobalt-chromium-tungsten nickel alloy which combines excellent high temperature strength and oxidation resistance to 2000°F with good resistance to sulfidation, wear and galling. Alloy L-605 / Haynes 25 has good forming characteristics and is capable of being forged, hot worked or cold worked, althoug it does work-harden very rapidly so frequent intermediate annealing treatments are recommend for complex forming operations. Alloy 25 / L-605 can also be readily welded by most conventional welding methods using similar composition welding wire (AMS 5796) or coated electrodes (AMS 5797). Alloy L-605 / Haynes 25 is supplied solution heat treated in the range of 2150-2250°F and rapid air or water quenched to attain optimum properties. Alloy L-605 / Haynes 25 has many applications in military and commercial gas turbine engine components such as rings, blades and combustion chamber parts although for many modern engines it has largely been replaced by Alloy 188 or Alloy 230.
Haynes 25 Mechanical Properties
Material | Temperature °F | Yield Strength 0.2% | Tensile Strength | Elongation (%) | Hardness HB |
Extruded Bar | RT | 310 Mpa | 862 Mpa | 30 | 277 max |
Material | Thickness (inches) | Yield Strength 0.2% | Tensile Strength | Elongation (%) | Hardness HRC |
Alloy 25 / L-605 | 0.005-0.020 | 55-80 | 130 | 30 | - |
Alloy 25 / L-605 | 0.020-0.032 | 55-80 | 130 | 35 | - |
Alloy 25 / L-605 | 0.032-0.043 | 55-80 | 130 | 40 | - |
Alloy 25 / L-605 | 0.043-0225 | 55-80 | 130 | 45 | - |
Haynes 25 Specifications
UNS R30605
AMS 5507 Sheet Strip and Plate
AMS 5759 Bar and Forging Stock
AMS 5796 Welding Wire
AMS 5797 (UNS W73605) Welding Rod
ASTM F90 Bar and Wire (surgical implant quality)
GE B50T26
GE B50A460
Tradenames: Udimet Alloy L-605, Haynes 25, Nickelvac L-605
The Haynes 25 items which we can manufacture and supply are the followings.
Haynes 25 Rod
3D printing spherical powder Haynes 25
Haynes 25 Rings
Haynes 25 Forgings
Haynes 25 pipe
Haynes 25 tube
Haynes 25 bars
Haynes 25 plates
Haynes 25 sheets
Haynes 25 Strip
Haynes 25 wire
Haynes 25 fitting Union
Haynes 25 Pipe Elbows
Haynes 25 PIPE Tee
Haynes 25 ADAPTERS
Haynes 25 pipe bend
Haynes 25 reducers
Haynes 25 fitting caps
Haynes 25 pipe outlets
Haynes 25 Stub Ends
Haynes 25 Couplings
Haynes 25 pipe Nipples
Haynes 25 BUSHINGS
Haynes 25 pipes sockets
Haynes 25 Pipe Gasket
Haynes 25 pipe joints
Haynes 25 pipe Cross
Haynes 25 Pipe Wyes
Haynes 25 seal ring
Haynes 25 Flange
Haynes 25 bolts
Haynes 25 nuts
ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN SMICO
SELECT SMICO, YOU WILL BE RIGHT
For more info and price of Haynes 25, please send us inquiry and you will have quick reply soon.
- Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Reliable 3d Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Welded Pipes Erw Steel Pipes Efw Steel Pipes Round Square Rectangular 1 Pieces / (Min. Order)
- Reliable 3d Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- SMICO Superior Galvanized Steel Pipes Galvanized Pipe Fittings 1 Pieces / (Min. Order)
- Solid Cra Clad Lined Pipes Cra Clad Pipes Api 5lc Clad Pipes Api 5ld Clad Pipes 1 Pieces / (Min. Order)
- Excellent Titanium Alloy 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Trustable 3d Printing Spherical Powder Magnesium Alloy Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Small Diameter Cold Drawn Semaless Steel Tubes 1 Pieces / (Min. Order)
- Large Diameter Hot Expanded Seamless Steel Pipes 1 Pieces / (Min. Order)
- The Best Quality Hot Rolled Seamless Steel Pipes Thick Wall Seamless Steel Pipe 1 Pieces / (Min. Order)