We are leading manufacturer and stockiest of Inconel 725 in China.
Inconel 725 Technical Data Sheet
Inconel 725 Chemical Composition Limits | ||||||||||||
Weight% | Ni | Cr | Mo | Nb | Ti | Al | C | Mn | Si | P | S | Fe |
Alloy 725 | 55.0-59.0 | 19.0 -22.5 | 7.0-9.5 | 2.75-4.0 | 1.0-1.7 | 0.35 max | 0.03 max | 0.35 max | 0.20 max | 0.015 max | 0.010 max | Rem |
Inconel 725 (UNS N07725) is a nickel-chromium-molybdenum-niobium alloy that is highly resistant to corrosion and has been age hardened for extremely high strength twice that of annealed alloy 625. Inconel 725 strength is developed by heat treatment rather than by cold work this also enables strength to be imparted to large non-uniform sections that cannot be strengthened by cold works. Inconel 725 is used for hangers, landing nipples and high strength fasteners in marine applications.
Inconel 725 Mechanical Properties
Material | Form and Condition | Yield Strength (0.2% Offset) | Tensile Strength | Elongation % | Hardness, Rc | ||
ksi | MPa | ksi | MPa | ||||
Alloy 725 round | Annealed | 62.0 | 427 | 124.0 | 855 | 57 | 5 |
Alloy 725 round | Age Hardened | 133.0 | 917 | 180.0 | 1241 | 30 | 36 |
Transverse Specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190mm) diameter |
Inconel 725 Specifications
Bar and Wire ASTM B 805, ASME Code Case 2217
Bar and Forging Stock SMC Specification HA91, ASME Code Case 2217
UNS N07725
FMC Spec M40504
NACE MR-0175/ ISO 15156
Inconel 725 (trademark)
Alloy Nickel Alloy 706 Inconel 706
Alloy Nickel Alloy 718 Inconel 718
Alloy 722
Inconel 722
UNS N07722
AMS 5541 Sheet and Strip
AMS 5714 Bar and Forgings
UNS N07718
Werkstoff Nr 2.4668
AMS 5596 Sheet, Strip and Plate
AMS 5597 Sheet, Strip and Plate
AMS 5589 Seamless Tube
AMS 5590 Seamless Tube
AMS 5662 Bars, Forgings and Rings
AMS 5663 Bars, Forgings and Rings
AMS 5664 Bars, Forgings and Rings
AMS 5832 Welding Wire
ASTM B637 Forgings
ASTM B670 Plate, Sheet and Strip
AFNOR NC 19 Fe Nb,
MSRR 7115 and MSRR 7116
Inconel 718 (trademark)
FMC Spec M40110, M40118, M40125, M40902, M40908, M40909, M40910
NACE MR-0175/ISO 15156
UNS N09706
AMS 5701
AMS 5702
AMS 5703
Inconel 706 (tradename)
The Inconel 725 items which we can manufacture and supply are the followings.
Inconel 725 Rod
3D printing spherical powder Inconel 725
Inconel 725 Rings
Inconel 725 Forgings
Inconel 725 pipe
Inconel 725 tube
Inconel 725 bars
Inconel 725 plates
Inconel 725 sheets
Inconel 725 Strip
Inconel 725 wire
Inconel 725 fitting Union
Inconel 725 Pipe Elbows
Inconel 725 PIPE Tee
Inconel 725 ADAPTERS
Inconel 725 pipe bend
Inconel 725 reducers
Inconel 725 fitting caps
Inconel 725 pipe outlets
Inconel 725 Stub Ends
Inconel 725 Couplings
Inconel 725 pipe Nipples
Inconel 725 BUSHINGS
Inconel 725 pipes sockets
Inconel 725 Pipe Gasket
Inconel 725 pipe joints
Inconel 725 pipe Cross
Inconel 725 Pipe Wyes
Inconel 725 seal ring
Inconel 725 Flange
Inconel 725 bolts
Inconel 725 nuts
Inconel X750 Rod
3D printing spherical powder Inconel X750
Inconel X750 Rings
Inconel X750 Forgings
Inconel X750 pipe
Inconel X750 tube
Inconel X750 bars
Inconel X750 plates
Inconel X750 sheets
Inconel X750 Strip
Inconel X750 wire
Inconel X750 fitting Union
Inconel X750 Pipe Elbows
Inconel X750 PIPE Tee
Inconel X750 ADAPTERS
Inconel X750 pipe bend
Inconel X750 reducers
Inconel X750 fitting caps
Inconel X750 pipe outlets
Inconel X750 Stub Ends
Inconel X750 Couplings
Inconel X750 pipe Nipples
Inconel X750 BUSHINGS
Inconel X750 pipes sockets
Inconel X750 Pipe Gasket
Inconel X750 pipe joints
Inconel X750 pipe Cross
Inconel X750 Pipe Wyes
Inconel X750 seal ring
Inconel X750 Flange
Inconel X750 bolts
Inconel X750 nuts
ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN SMICO
SELECT SMICO, YOU WILL BE RIGHT
For more info and price of Inconel 725, please send us inquiry and you will have quick reply soon.
- 3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- 3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Welded Pipes Erw Steel Pipes Efw Steel Pipes Round Square Rectangular 1 Pieces / (Min. Order)
- SMICO Superior Galvanized Steel Pipes Galvanized Pipe Fittings 1 Pieces / (Min. Order)
- Solid Cra Clad Lined Pipes Cra Clad Pipes Api 5lc Clad Pipes Api 5ld Clad Pipes 1 Pieces / (Min. Order)
- Excellent Titanium Alloy 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Trustable 3d Printing Spherical Powder Magnesium Alloy Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Small Diameter Cold Drawn Semaless Steel Tubes 1 Pieces / (Min. Order)
- Large Diameter Hot Expanded Seamless Steel Pipes 1 Pieces / (Min. Order)
- The Best Quality Hot Rolled Seamless Steel Pipes Thick Wall Seamless Steel Pipe 1 Pieces / (Min. Order)