SMICO Superior Galvanized Steel Pipes Galvanized Pipe Fittings
-
Payment
-
Origin
China Mainland
-
Minimum Order
1
-
Packing
Pieces
- Contact Now Start Order
- Description
Product Detail
We are leading manufacturer and stockiest of Galvanized steel pipes in China.
Galvanized steel pipes Class Light Galvanized Steel Pipe | ||||||||
Nominal | Designation | Outside Diameter | Wall | Calculated Weight | Threads | Number | ||
Min | Max | Plain Ends | Threads&Coupling | |||||
15 | 1/2 | 21.0 | 21.4 | 2.0 | 0.947 | 0.956 | 14 | 169 |
20 | 3/4 | 26.4 | 26.9 | 2.3 | 1.38 | 1.39 | 14 | 127 |
25 | 1 | 33.2 | 33.8 | 2.6 | 1.98 | 2.00 | 11 | 91 |
32 | 1 1/4 | 41.9 | 42.5 | 2.6 | 2.54 | 2.57 | 11 | 61 |
40 | 1 1/2 | 47.8 | 48.4 | 2.9 | 3.23 | 3.27 | 11 | 44 |
50 | 2 | 59.6 | 60.2 | 2.9 | 4.08 | 4.15 | 11 | 37 |
65 | 2 1/2 | 75.2 | 76.0 | 3.2 | 5.71 | 5.83 | 11 | 24 |
80 | 3 | 87.9 | 88.7 | 3.2 | 6.72 | 6.89 | 11 | 19 |
100 | 4 | 113.0 | 113.9 | 3.6 | 9.75 | 10.00 | 11 | 14 |
Galvanized steel pipes sizes
WT: 0.25mm-75mm.
OD: 15mm-720mm.
LR: 6M OR 12M
TYPE: Seamless pipe and Welded steel pipe (galvanized pipe,ms pipe and black steel pipe)
The seamless tubes included into the item list that conducively offer a wide range of choice no matter if for production or application.
STANDARD | Galvanized steel pipes CHEMICAL COMPOSITION | Galvanized steel pipes MECHANICAL PROPERTIES | Galvanized steel pipes Hydrostatic | |||||
C | Mn | P | S | Yield | Tensile | Elongation | ||
Max% | Max% | Max% | Max% | (Min) | (Min) | (Min) | (Bar) | |
Class Light | 0.20 | 1.20 | 0.045 | 0.045 | 195 | 320-460 | 20 | 50 |
Class Medium | 0.20 | 1.20 | 0.045 | 0.045 | 195 | 320-460 | 20 | 50 |
Class Heavy | 0.20 | 1.20 | 0.045 | 0.045 | 195 | 320-460 | 20 | 50 |
Galvanized steel pipes Class Medium Galvanized Steel Pipe | ||||||||
Nominal | Designation | Outside Diameter | Wall | Calculated Weight | Threads | Number | ||
Min | Max | Plain Ends | Threads&Coupling | |||||
15 | 1/2 | 21.1 | 21.7 | 2.6 | 1.21 | 1.22 | 14 | 169 |
20 | 3/4 | 26.6 | 27.2 | 2.6 | 1.56 | 1.57 | 14 | 127 |
25 | 1 | 33.4 | 34.2 | 3.2 | 2.41 | 2.43 | 11 | 91 |
32 | 1 1/4 | 42.1 | 42.9 | 3.2 | 3.10 | 3.13 | 11 | 61 |
40 | 1 1/2 | 48.0 | 48.8 | 3.2 | 3.57 | 3.61 | 11 | 44 |
50 | 2 | 59.8 | 60.8 | 3.6 | 5.03 | 5.10 | 11 | 37 |
65 | 2 1/2 | 75.4 | 76.6 | 3.6 | 6.43 | 6.55 | 11 | 24 |
80 | 3 | 88.1 | 89.5 | 4.0 | 8.37 | 8.54 | 11 | 19 |
100 | 4 | 113.1 | 114.9 | 4.5 | 12.20 | 12.50 | 11 | 14 |
125 | 5 | 138.7 | 140.6 | 5.0 | 16.60 | 17.10 | 11 | 7 |
150 | 6 | 164.1 | 166.1 | 5.0 | 19.70 | 20.30 | 11 | 7 |
Galvanized steel pipes Class Heavy Galvanized Steel Pipe | ||||||||
Nominal | Designation | Outside Diameter | Wall | Calculated Weight | Threads | Number | ||
Min | Max | Plain Ends | Threads&Coupling | |||||
15 | 1/2 | 21.1 | 21.7 | 3.2 | 1.44 | 1.45 | 14 | 169 |
20 | 3/4 | 26.6 | 27.2 | 3.2 | 1.87 | 1.88 | 14 | 127 |
25 | 1 | 33.4 | 34.2 | 4.0 | 2.94 | 2.96 | 11 | 91 |
32 | 1 1/4 | 42.1 | 42.9 | 4.0 | 3.8 | 3.83 | 11 | 61 |
40 | 1 1/2 | 48.0 | 48.8 | 4.0 | 4.38 | 4.42 | 11 | 44 |
50 | 2 | 59.8 | 60.8 | 4.5 | 6.19 | 6.26 | 11 | 37 |
65 | 2 1/2 | 75.4 | 76.6 | 4.5 | 7.93 | 8.05 | 11 | 24 |
80 | 3 | 88.1 | 89.5 | 5.0 | 10.30 | 10.50 | 11 | 19 |
100 | 4 | 113.3 | 114.9 | 5.4 | 14.50 | 14.80 | 11 | 14 |
125 | 5 | 138.7 | 140.6 | 5.4 | 17.90 | 18.40 | 11 | 7 |
150 | 6 | 164.1 | 166.1 | 5.4 | 21.30 | 21.90 | 11 | 7 |
· Supplied in a galvanized finish.
· Available as cut lengths, full bars or bundles - please contact our Sales Dept. for quotation and carriage rates.
· 26.9mm, 33.7mm, 42.4mm, 48.3mm and 60.3mm sizes available to suit many of our tubular fittings.
· Also available 48.3mm x 4mm O/D tube to BS 1139 (Scaffold).
Nominal bore | Outside diameter | Thickness | Mass | ||||||
Light | Medium/ | Light | Medium | Heavy | Light | Medium | Heavy | ||
in | mm | mm | mm | mm | mm | mm | kg/m | kg/m | kg/m |
1/4 | 8 | 13.60 | 13.90 | 1.80 | 2.30 | 2.90 | 0.515 | 0.641 | 0.765 |
3/8 | 10 | 17.10 | 17.40 | 1.80 | 2.30 | 2.90 | 0.670 | 0.839 | 1.020 |
1/2 | 15 | 21.40 | 21.70 | 2.00 | 2.60 | 3.20 | 0.947 | 1.210 | 1.440 |
3/4 | 20 | 26.90 | 27.20 | 2.30 | 2.60 | 3.20 | 1.380 | 1.560 | 1.870 |
1 | 25 | 33.80 | 34.20 | 2.60 | 3.20 | 4.00 | 1.980 | 2.410 | 2.940 |
1 1/4 | 32 | 42.50 | 42.90 | 2.60 | 3.20 | 4.00 | 2.540 | 3.100 | 3.800 |
1 1/2 | 40 | 48.40 | 48.80 | 2.90 | 3.20 | 4.00 | 3.230 | 3.570 | 4.380 |
2 | 50 | 60.20 | 60.80 | 2.90 | 3.60 | 4.50 | 4.080 | 5.030 | 6.190 |
2 1/2 | 65 | 76.00 | 76.60 | 3.20 | 3.60 | 4.50 | 5.710 | 6.430 | 7.930 |
3 | 80 | 88.70 | 89.50 | 3.20 | 4.00 | 5.00 | 6.720 | 8.370 | 10.300 |
4 | 100 | 113.90 | 114.90 | 3.60 | 4.50 | 5.40 | 9.750 | 12.200 | 14.500 |
5 | 125 | 140.60 | 5.00 | 5.40 | 16.600 | 17.900 | |||
6 | 150 | 166.10 | 5.00 | 5.40 |
ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN SMICO
SELECT SMICO, YOU WILL BE RIGHT
For more info and price of Galvanized steel pipes, please send us inquiry and you will have quick reply soon.
- Solid Cra Clad Lined Pipes Cra Clad Pipes Api 5lc Clad Pipes Api 5ld Clad Pipes 1 Pieces / (Min. Order)
- Small Diameter Cold Drawn Semaless Steel Tubes 1 Pieces / (Min. Order)
- Large Diameter Hot Expanded Seamless Steel Pipes 1 Pieces / (Min. Order)
- The Best Quality Hot Rolled Seamless Steel Pipes Thick Wall Seamless Steel Pipe 1 Pieces / (Min. Order)