We are leading manufacturer and stockiest of Magnesium alloy in China.
Magnesium alloy AZ31B
Magnesium alloy AZ31B Technical Data Sheet
Magnesium alloy AZ31B Chemical Composition Limits | ||||||||||
Weight % | Al | Zn | Mn | Si | Cu | Ca | Fe | Ni | Others | Mg |
Magnesium | 2.5 - 3.5 | 0.7 - 1.3 | 0.2 min | 0.05 max | 0.05 max | 0.04 max | 0.005 max | 0.005 max | 0.30 max total | bal |
Magnesium alloy AZ31B is a wrought magnesium alloy with good room-temperature strength and ductility combined with corrosion resistance and weldability. AZ31B finds application in wide variety of uses including aircraft fuselages, cell phone and laptop cases, speaker cones and concrete tools. Magnesium alloy AZ31B can be superformed at elevated temperatures to produce a wide variety of intricate components for automotive uses.
Magnesium alloy AZ31B is also available as tooling plate which is specially produced to provide a flat plate surface. The production process of Magnesium alloy AZ31B-TP also results in plate with exceptional dimensional stability in machining. This allows for the manufacture of very complex parts but also components which benefit from the dimensional stability such as jigs, fixtures, optical benches, vibration test equipment and inspection gauges.
Magnesium alloy AZ31B Mechanical Properties
Material | Condition | Thickness " | Tensile Strength | Yield Strength 0.2 % | Elongation in 4D (%) |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 0.016 - 0.249 | 39 | 29 | 6 |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 0.249 - 0.374 | 38 | 26 | 8 |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 0.374 - 0.500 | 37 | 24 | 8 |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 0.500 - 1.00 | 36 | 22 | 8 |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 1.00 - 2.00 | 34 | 20 | 8 |
Magnesium alloy AZ31B Sheet | Cold Rolled, partially annealed | 2.00 - 3.00 | 34 | 18 | 8 |
Magnesium alloy AZ31B | Tooling Plate | 35 | 19 | 10 | |
Tooling Plate properties are typical only and are not guaranteed or reported. |
Magnesium alloy AZ31B characteristics
35% Lighter than Aluminum.
1 on 15 people in Europe need a mobility aid.
Breakthrough in magnesium technologies has resulted in the start for new lightweight mobility aids.
Less weight, more comfort and affordable.
Magnesium parts for Aerospace, Automotive,
Defense, General machinery, etc. has help reduce weight and increase efficiency.
Most magnesium alloys are not heat treatable like Aluminum.
Magnesium alloy AZ31B Specifications
AMS 4375 - AZ31B-O Sheet, plate
AMS 4376 - AZ31B-H26 Plate
AMS 4377 - AZ31B-H24 Sheet, plate
AMS 4382 - AZ31B-O Plate
ASTM B90
ASTM B107
QQ-M-44B
QQ-M-31B
BS 3370 MAG-S-1110
BS 3370 MAG-E-111M
Werkstoff W.3504 (aerospace)
Werkstoff WS 3.5312
French Commercial - F3
French Aerospace- AIR/AFNOR G-A3Z1
EN1753 MG-P-62
The Magnesium alloy AZ31B items which we can manufacture and supply are the followings.
Magnesium alloy AZ31B Rod
3D printing spherical powder Magnesium
Magnesium alloy AZ31B Rings
Magnesium alloy AZ31B Forgings
Magnesium alloy AZ31B pipe
Magnesium alloy AZ31B tube
Magnesium alloy AZ31B bars
Magnesium alloy AZ31B plates
Magnesium alloy AZ31B sheets
Magnesium alloy AZ31B Strip
Magnesium alloy AZ31B wire
Magnesium alloy AZ31B fitting Union
Magnesium alloy AZ31B Pipe Elbows
Magnesium alloy AZ31B PIPE Tee
Magnesium alloy AZ31B ADAPTERS
Magnesium alloy AZ31B pipe bend
Magnesium alloy AZ31B reducers
Magnesium alloy AZ31B fitting caps
Magnesium alloy AZ31B pipe outlets
Magnesium alloy AZ31B Stub Ends
Magnesium alloy AZ31B Couplings
Magnesium alloy AZ31B pipe Nipples
Magnesium alloy AZ31B BUSHINGS
Magnesium alloy AZ31B pipes sockets
Magnesium alloy AZ31B Pipe Gasket
Magnesium alloy AZ31B pipe joints
Magnesium alloy AZ31B pipe Cross
Magnesium alloy AZ31B Pipe Wyes
Magnesium alloy AZ31B seal ring
Magnesium alloy AZ31B Flange
Magnesium alloy AZ31B bolts
Magnesium alloy AZ31B nuts
Magnesium alloy AZ61A
Magnesium alloy AZ61A Technical Data Sheet
Magnesium alloy AZ61A Chemical Composition Limits | ||||||||
Weight % | Al | Zn | Mn | Zr | Th | Rare Earth | Other | Specific Gravity |
Magnesium | 6.5 | 1.0 | 0.15 | - | - | - | - | 1.80 |
Magnesium alloy AZ61A (AZM) is a general purpose magnesium alloy which is both gas and arc weldable. AZ61A has a higher tensile strength and superior corrosion resistance compared to AZ31B and it is possible to perform various finishing on its surface.
Magnesium alloy AZ61A Mechanical Properties
Material | Diameter | Ultimate Tensile Strength | Yield Strength | Elongation |
Magnesium alloy AZ61A-F Round Bar | =0.25" | 46 | 33 | 17 |
Magnesium alloy AZ61A-F Round Bar | 0.25" - 2.5" | 45 | 33 | 16 |
Magnesium alloy AZ61A-F Round Bar | 2.5" - 5.0" | 45 | 31 | 15 |
Magnesium alloy AZ61A characteristics
35% Lighter than Aluminum.
1 on 15 people in Europe need a mobility aid.
Breakthrough in magnesium technologies has resulted in the start for new lightweight mobility aids.
Less weight, more comfort and affordable.
Magnesium parts for Aerospace, Automotive,
Defense, General machinery, etc. has help reduce weight and increase efficiency.
Most magnesium alloys are not heat treatable like Aluminum.
Magnesium alloy AZ61A Specifications
BS 2L503 - Tube
BS L512 - Bar
BS L513 - Forgings
BS 3373 MAG-E-121M
BS 3372 MAG-E-121M
AMS 4350 AZ61A-F extrusions
QQ-M-31B
QQ-M-40B
WW-T-825B
ASTM B107
ASTM B91
Werkstoff W.3510 (aerospace)
Werkstoff 3.5612
French Commercial: M1
French Aerospace: AIR/AFNOR G-A6Z1
European / AECMA: EN 1753 MG-P-63
The Magnesium alloy AZ61A items which we can manufacture and supply are the followings.
Magnesium alloy AZ61A Rod
Magnesium alloy AZ61A Rings
Magnesium alloy AZ61A Forgings
Magnesium alloy AZ61A pipe
Magnesium alloy AZ61A tube
Magnesium alloy AZ61A bars
Magnesium alloy AZ61A plates
Magnesium alloy AZ61A sheets
Magnesium alloy AZ61A Strip
Magnesium alloy AZ61A wire
Magnesium alloy AZ61A fitting Union
Magnesium alloy AZ61A Pipe Elbows
Magnesium alloy AZ61A PIPE Tee
Magnesium alloy AZ61A ADAPTERS
Magnesium alloy AZ61A pipe bend
Magnesium alloy AZ61A reducers
Magnesium alloy AZ61A fitting caps
Magnesium alloy AZ61A pipe outlets
Magnesium alloy AZ61A Stub Ends
Magnesium alloy AZ61A Couplings
Magnesium alloy AZ61A pipe Nipples
Magnesium alloy AZ61A BUSHINGS
Magnesium alloy AZ61A pipes sockets
Magnesium alloy AZ61A Pipe Gasket
Magnesium alloy AZ61A pipe joints
Magnesium alloy AZ61A pipe Cross
Magnesium alloy AZ61A Pipe Wyes
Magnesium alloy AZ61A seal ring
Magnesium alloy AZ61A Flange
Magnesium alloy AZ61A bolts
Magnesium alloy AZ61A nuts
Magnesium alloy AZ80A
Magnesium alloy AZ92A
Magnesium alloy EZ33A
Magnesium alloy EZ33A Technical Data Sheet
Magnesium alloy EZ33A Chemical Composition Limits | |||||
Weight % | Rare Earth | Zn | Zr Total | Others Total | Mg |
Magnesium Alloy | 2.5 - 4.0 | 2.0 - 3 | 0.45 - 1.0 | 0.30 max | Bal |
Magnesium alloy EZ33A Specifications
BS 2L126 Castings
BS 2970 MAG6-TE
ASTM B80
QQ-M-56B
AMS 4442 - EZ33A-T5 sand castings
AMS 4396 - EZ33A welding wire
MIL-R-6944
Werkstoff WS 3.6204 (aerospace)
Werkstoff WS 3.5103
French Commercial: ZRE1
French Aerospace: AIR/AFNOR G-TR3Z2
European Specification: EN 1753 EN-MN65120
The Magnesium alloy EZ33A items which we can manufacture and supply are the followings.
Magnesium alloy EZ33A Rod
Magnesium alloy EZ33A Rings
Magnesium alloy EZ33A Forgings
Magnesium alloy EZ33A pipe
Magnesium alloy EZ33A tube
Magnesium alloy EZ33A bars
Magnesium alloy EZ33A plates
Magnesium alloy EZ33A sheets
Magnesium alloy EZ33A Strip
Magnesium alloy EZ33A wire
Magnesium alloy EZ33A fitting Union
Magnesium alloy EZ33A Pipe Elbows
Magnesium alloy EZ33A PIPE Tee
Magnesium alloy EZ33A ADAPTERS
Magnesium alloy EZ33A pipe bend
Magnesium alloy EZ33A reducers
Magnesium alloy EZ33A fitting caps
Magnesium alloy EZ33A pipe outlets
Magnesium alloy EZ33A Stub Ends
Magnesium alloy EZ33A Couplings
Magnesium alloy EZ33A pipe Nipples
Magnesium alloy EZ33A BUSHINGS
Magnesium alloy EZ33A pipes sockets
Magnesium alloy EZ33A Pipe Gasket
Magnesium alloy EZ33A pipe joints
Magnesium alloy EZ33A pipe Cross
Magnesium alloy EZ33A Pipe Wyes
Magnesium alloy EZ33A seal ring
Magnesium alloy EZ33A Flange
Magnesium alloy EZ33A bolts
Magnesium alloy EZ33A nuts
Magnesium Alloy HK31A
Magnesium alloy ZK60A
Magnesium alloy ZK60A Technical Data Sheet
Magnesium alloy ZK60AChemical Composition Limits | ||||||||
Weight % | Al | Zn | Mn | Zr | Th | Rare Earth | Other | Specific Gravity |
Magnesium | - | 4.8 - 6.2 | - | 0.45 (min) | - | - | 0.30 | 1.83 |
Magnesium alloy ZK60A Mechanical Properties
Material | Cross-Sectional area (sq in) | Tensile Strength (ksi) | Yield Strength (ksi) | Elongation 4D |
Magnesium alloy ZK60A - T5 Bar | < 5 | 45 | 36 | 4 |
Magnesium alloy ZK60A - T5 Bar | 5 - 25 | 45 | 34 | 6 |
Magnesium alloy ZK60A - T5 Bar | 25 - 40 | 43 | 31 | 6 |
Magnesium alloy ZK60A Specifications
AMS 4352 - ZK60A-T5 Extrusions
AMS 4362 - ZK60A-T5 Forgings
UNS M16600
ASTM B107
ASTM B191
ASTM E8
The Magnesium alloy ZK60A items which we can manufacture and supply are the followings.
Magnesium alloy ZK60A Rod
Magnesium alloy ZK60A Rings
Magnesium alloy ZK60A Forgings
Magnesium alloy ZK60A pipe
Magnesium alloy ZK60A tube
Magnesium alloy ZK60A bars
Magnesium alloy ZK60A plates
Magnesium alloy ZK60A sheets
Magnesium alloy ZK60A Strip
Magnesium alloy ZK60A wire
Magnesium alloy ZK60A fitting Union
Magnesium alloy ZK60A Pipe Elbows
Magnesium alloy ZK60A PIPE Tee
Magnesium alloy ZK60A ADAPTERS
Magnesium alloy ZK60A pipe bend
Magnesium alloy ZK60A reducers
Magnesium alloy ZK60A fitting caps
Magnesium alloy ZK60A pipe outlets
Magnesium alloy ZK60A Stub Ends
Magnesium alloy ZK60A Couplings
Magnesium alloy ZK60A pipe Nipples
Magnesium alloy ZK60A BUSHINGS
Magnesium alloy ZK60A pipes sockets
Magnesium alloy ZK60A Pipe Gasket
Magnesium alloy ZK60A pipe joints
Magnesium alloy ZK60A pipe Cross
Magnesium alloy ZK60A Pipe Wyes
Magnesium alloy ZK60A seal ring
Magnesium alloy ZK60A Flange
Magnesium alloy ZK60A bolts
Magnesium alloy ZK60A nuts
Magnesium alloy HM31A
Magnesium alloy HM31A Technical Data Sheet
Magnesium alloy HM31A Chemical Composition Limits | ||||||||
Weight % | Al | Zn | Mn | Zr | Th | Rare Earth | Other | Specific Gravity |
Magnesium Alloy | - | - | 1.2 min | - | 2.5 - 3.5 | - | 0.30 | 1.81 |
Magnesium alloy HM31A Specifications
AMS 4388 - HM31A-F Extrusions
AMS 4389 - HM31A - T5 Extrusions (precipitation heat treated)
MIL-M-8915
The Magnesium alloy HM31A items which we can manufacture and supply are the followings.
Magnesium alloy HM31A Rod
Magnesium alloy HM31A Rings
Magnesium alloy HM31A Forgings
Magnesium alloy HM31A pipe
Magnesium alloy HM31A tube
Magnesium alloy HM31A bars
Magnesium alloy HM31A plates
Magnesium alloy HM31A sheets
Magnesium alloy HM31A Strip
Magnesium alloy HM31A wire
Magnesium alloy HM31A fitting Union
Magnesium alloy HM31A Pipe Elbows
Magnesium alloy HM31A PIPE Tee
Magnesium alloy HM31A ADAPTERS
Magnesium alloy HM31A pipe bend
Magnesium alloy HM31A reducers
Magnesium alloy HM31A fitting caps
Magnesium alloy HM31A pipe outlets
Magnesium alloy HM31A Stub Ends
Magnesium alloy HM31A Couplings
Magnesium alloy HM31A pipe Nipples
Magnesium alloy HM31A BUSHINGS
Magnesium alloy HM31A pipes sockets
Magnesium alloy HM31A Pipe Gasket
Magnesium alloy HM31A pipe joints
Magnesium alloy HM31A pipe Cross
Magnesium alloy HM31A Pipe Wyes
Magnesium alloy HM31A seal ring
Magnesium alloy HM31A Flange
Magnesium alloy HM31A bolts
Magnesium alloy HM31A nuts
Magnesium alloy HM21A
Magnesium alloy ZE41
Magnesium Alloy ZK21
Magnesium alloy ZK60A
Magnesium alloy ZK60 Technical Data Sheet
Magnesium alloy ZK60 Chemical Composition Limits | ||||||||
Weight % | Al | Zn | Mn | Zr | Th | Rare Earth | Other | Specific Gravity |
Magnesium | - | 4.8 - 6.2 | - | 0.45 (min) | - | - | 0.30 | 1.83 |
Magnesium alloy ZK60 Mechanical Properties
Material | Cross-Sectional area (sq in) | Tensile Strength (ksi) | Yield Strength (ksi) | Elongation 4D |
Magnesium alloy ZK60A - T5 Bar | < 5 | 45 | 36 | 4 |
Magnesium alloy ZK60A - T5 Bar | 5 - 25 | 45 | 34 | 6 |
Magnesium alloy ZK60A - T5 Bar | 25 - 40 | 43 | 31 | 6 |
Magnesium alloy ZK60 Specifications
AMS 4352 - ZK60A-T5 Extrusions
AMS 4362 - ZK60A-T5 Forgings
UNS M16600
ASTM B107
ASTM B191
ASTM E8
The Magnesium alloy ZK60 items which we can manufacture and supply are the followings.
Magnesium alloy ZK60 Rod
Magnesium alloy ZK60 Rings
Magnesium alloy ZK60 Forgings
Magnesium alloy ZK60 pipe
Magnesium alloy ZK60 tube
Magnesium alloy ZK60 bars
Magnesium alloy ZK60 plates
Magnesium alloy ZK60 sheets
Magnesium alloy ZK60 Strip
Magnesium alloy ZK60 wire
Magnesium alloy ZK60 fitting Union
Magnesium alloy ZK60 Pipe Elbows
Magnesium alloy ZK60 PIPE Tee
Magnesium alloy ZK60 ADAPTERS
Magnesium alloy ZK60 pipe bend
Magnesium alloy ZK60 reducers
Magnesium alloy ZK60 fitting caps
Magnesium alloy ZK60 pipe outlets
Magnesium alloy ZK60 Stub Ends
Magnesium alloy ZK60 Couplings
Magnesium alloy ZK60 pipe Nipples
Magnesium alloy ZK60 BUSHINGS
Magnesium alloy ZK60 pipes sockets
Magnesium alloy ZK60 Pipe Gasket
Magnesium alloy ZK60 pipe joints
Magnesium alloy ZK60 pipe Cross
Magnesium alloy ZK60 Pipe Wyes
Magnesium alloy ZK60 seal ring
Magnesium alloy ZK60 Flange
Magnesium alloy ZK60 bolts
Magnesium alloy ZK60 nuts
ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN SMICO
SELECT SMICO, YOU WILL BE RIGHT
For more info and price of Magnesium alloy, please send us inquiry and you will have quick reply soon.
- Excellent Titanium Alloy 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- 3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Welded Pipes Erw Steel Pipes Efw Steel Pipes Round Square Rectangular 1 Pieces / (Min. Order)
- Reliable 3d Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- SMICO Superior Galvanized Steel Pipes Galvanized Pipe Fittings 1 Pieces / (Min. Order)
- Solid Cra Clad Lined Pipes Cra Clad Pipes Api 5lc Clad Pipes Api 5ld Clad Pipes 1 Pieces / (Min. Order)
- Excellent Titanium Alloy 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Small Diameter Cold Drawn Semaless Steel Tubes 1 Pieces / (Min. Order)
- Large Diameter Hot Expanded Seamless Steel Pipes 1 Pieces / (Min. Order)
- The Best Quality Hot Rolled Seamless Steel Pipes Thick Wall Seamless Steel Pipe 1 Pieces / (Min. Order)