Qualified 3d Printing Spherical Powder Inconel C276 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods
-
Payment
-
Origin
China Mainland
-
Minimum Order
1
-
Packing
Pieces
- Contact Now Start Order
- Description
Product Detail
We are leading manufacturer and stockist of Inconel C276 in China.
Inconel C276 Technical Data Sheet
Inconel C276 Chemical Composition Limits | ||||||||||||
Weight% | C | P | Si | Ni | Co | W | Mn | S | Cr | Mo | V | Fe |
C276 | 0.01 max | 0.040 max | 0.08 max | Bal | 2.5 max | 3-4.5 | 1.00 max | 0.030 max | 14.5-16.5 | 15-17 | 0.35 max | 4-7 |
Nickel Superalloy C276 is a nickel molybdenum chromium tungsten alloy with the addition of Tungsten. C276 has good fabricability and impressive corrosion resistance in some of the most severe environments. Due to C 276's properties it is commonly used in pollution control, chemical, petrochemical and waste incineration applications.
Inconel C276 Mechanical Properties
Material | Ultimate Tensile (min) | Yield Strength (Min) | Elongation % | Hardness Rb | ||
Ksi | Mpa | Ksi | Mpa | |||
C276 Tube | 105.4 | 727 | 45.4 | 313 | 70 | 92 |
C276 Plate | 107.4 | 741 | 50.3 | 347 | 67 | 89 |
C276 Bar | 110.0 | 758 | 52.6 | 363 | 62 | 88 |
C276 Sheet | 115.5 | 796 | 54.6 | 376 | 60 | 86 |
Inconel C276 Specifications
UNS N10276
AMS 5750 Bar, Forgings
WS 2.4819
ASTM B574, ASME SB574 Bar Products
ASTM B575, ASME SB575 Plate, Sheet and Strip
ASTM B619, ASME SB619 Welded Pipe
ASTM B622, ASME SB622 Seamless Tubing
ASTM B626, ASME SB 626 Welded Tubing
ASTM B366, ASME SB 366 Wrought Corrosion Resistant Fittings CR HC 276, Wrought ANSI Pressure Fitting-WPHC276
ASTM B564 Forgings
AWS A 5.14, ASME SA 5.14 Welding Wire (ER NiCrMo-4)
AWS A 5.11, ASME SA 5.11 Covered Electrodes (E NiCRMo-4)
NACE MR-01-75
Inconel C276 (trademark)
Similar Specifications
AMS 5750 (Hastelloy C, UNS N10002)
ASTM B751
Werkstoff Nr. 2.4819
DIN 17744, DIN 17750, DIN 17751 and DIN 17752,VRC276
The Inconel C276 items which we can manufacture and supply are the followings.
Inconel C276 Rod
3D printing spherical powder Incoloy C276
Inconel C276 Rings
Inconel C276 Forgings
Inconel C276 pipe
Inconel C276 tube
Inconel C276 bars
Inconel C276 plates
Inconel C276 sheets
Inconel C276 Strip
Inconel C276 wire
Inconel C276 fitting Union
Inconel C276 Pipe Elbows
Inconel C276 PIPE Tee
Inconel C276 ADAPTERS
Inconel C276 pipe bend
Inconel C276 reducers
Inconel C276 fitting caps
Inconel C276 pipe outlets
Inconel C276 Stub Ends
Inconel C276 Couplings
Inconel C276 pipe Nipples
Inconel C276 BUSHINGS
Inconel C276 pipes sockets
Inconel C276 Pipe Gasket
Inconel C276 pipe joints
Inconel C276 pipe Cross
Inconel C276 Pipe Wyes
Inconel C276 seal ring
Inconel C276 Flange
Inconel C276 bolts
Inconel C276 nuts
ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN SMICO
SELECT SMICO, YOU WILL BE RIGHT
For more info and price of Inconel C276 , please send us inquiry and you will have quick reply soon.
- 3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Reliable 3d Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- 3d Printing Spherical Powder Haynes 25 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Welded Pipes Erw Steel Pipes Efw Steel Pipes Round Square Rectangular 1 Pieces / (Min. Order)
- Reliable 3d Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- SMICO Superior Galvanized Steel Pipes Galvanized Pipe Fittings 1 Pieces / (Min. Order)
- Solid Cra Clad Lined Pipes Cra Clad Pipes Api 5lc Clad Pipes Api 5ld Clad Pipes 1 Pieces / (Min. Order)
- Excellent Titanium Alloy 3d Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Trustable 3d Printing Spherical Powder Magnesium Alloy Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods 1 Pieces / (Min. Order)
- Small Diameter Cold Drawn Semaless Steel Tubes 1 Pieces / (Min. Order)
- Large Diameter Hot Expanded Seamless Steel Pipes 1 Pieces / (Min. Order)
- The Best Quality Hot Rolled Seamless Steel Pipes Thick Wall Seamless Steel Pipe 1 Pieces / (Min. Order)